Glass bottle consumption will sometimes be sick when the cork inside diameter is small (also known as loan mouth / fine mouth) condition, loan mouth is also two kinds, one is all mouth inside diameter average value reduction, there is also a kind of partial reduction; detection when applying standard iron bar or internal plug into the bottle cork inside, part of the block or a little can not get down; cause this kind of condition and three factors have a relationship: feeder material shape and mold temperature, mandrel design program and The actual operation, the actual operation of the consumer.


Feeder material shape and mold temperature --- material drop shape design head is very sharp too fine, material drop temperature uneven value or too high are caused by the glass bottle loan mouth; solution is to adjust the drop material shape to arrive at a suitable specification level, the application of acute bronchitis to the feeder drop temperature reduction to a suitable temperature; in the mandrel design program when the product shape design is not scientific is also very easy to cause fine mouth, consumption when the oil stains are too large or with tempered laminated glass Material touching time is too long and too short, which in turn leads to the mandrel temperature is slightly lower will lead to loan mouth.
This requires the actual operation of the work of the staff diligently check, once found that the oil stains are large immediately settle; consumption of the actual operation of the bottle tongs application is unreasonable will also cause loan mouth, if the bottle tongs become small, the head and neck of the glass bottle will be clamped flat, the cork within the unique will of course shrink; so in the actual operation before the heart accurately measure the cork type specifications, select the appropriate bottle tongs is also very important.
Other problems if only as the first glimpse of the mold mouth cooler application is unreasonable or blowing check head spacing corks too high too clumsy will also cause loan mouth problems, such are stipulated in the actual operation of the master or varnish material workers diligent thermal inspection, proper disposal of problems properly handled to avoid the development of long-term large hazards, glass bottle manufacturers once caused by loan mouth or fine mouth problems, rushed to consumer manufacturers in the canning, will be sick canning deviation Bottle stopper management office can not be successfully canned.
Some bottle stopper inner diameter is too thin, the canning tube basically can not insert into the bottle stopper leading to not canning; in the engine cover, if the bottle stopper public service facility has an inner plug, it will lead to the bottle stopper inner diameter and the original establishment of the inner plug does not match, also some even if the cork pressed into the bottle stopper internal, because the loan mouth leads to the inner plug back popped out, and finally are sick liquid leakage or oozing liquid condition.

 