1. The internal pressure resistance shall be carried out according to the provisions of GB 4546.
2. Thermal shock resistance shall be carried out in accordance with the provisions of GB 4547.
3. The internal stress shall be carried out in accordance with the provisions of GB 4545.
4. The water erosion resistance of the inner surface shall be in accordance with the provisions of GB 4548.
5. Impact resistance shall be carried out in accordance with the provisions of GB 6552. The impact point is located in the middle of the bottle during the test.